ScholarGate
어시스턴트

방법 비교

선택한 방법을 나란히 검토하세요. 서로 다른 행은 강조 표시됩니다.

얀카 경도×나무 수축×
분야임학임학
계열Process / pipelineProcess / pipeline
기원 연도19341950
창시자Gabriel JankaCarl Skaar
유형hardness testmoisture response test
원전ASTM D1037-21. (2021). Standard test methods for evaluating properties of wood-base fiber and particle panel materials. ASTM International. link ↗ASTM D143-19. (2019). Standard test methods for small clear specimens of timber. ASTM International. link ↗
별칭wood hardness, resistance to indentationdimensional change, anisotropic shrinkage
관련32
요약The Janka hardness test measures wood resistance to indentation and denting by forcing a steel ball into the wood surface under standard load. Developed by Gabriel Janka in 1934, the test is a simple, nondestructive indicator of wood durability, wear resistance, and suitability for flooring, furniture, and other wear-prone applications. Janka hardness is one of the most widely used wood property metrics in wood science and commerce.Wood shrinkage is the dimensional change that occurs as wood loses moisture from green (freshly felled) to oven-dry condition. Wood shrinks anisotropically: tangentially (along growth rings) more than radially (from center to edge), and both more than longitudinally (along the grain). Measuring shrinkage percentages is essential for understanding wood drying behavior, predicting checking and warping, and selecting materials for applications sensitive to dimensional change (flooring, cabinetry, musical instruments).
ScholarGate데이터셋
  1. v1
  2. 2 출처
  3. PUBLISHED
  1. v1
  2. 2 출처
  3. PUBLISHED

검색으로 이동 슬라이드 다운로드