ScholarGate
Assistente

Comparar métodos

Examine os métodos selecionados lado a lado; as linhas que diferem ficam destacadas.

Encolhimento da Madeira×Dureza Janka×
ÁreaCiências florestaisCiências florestais
FamíliaProcess / pipelineProcess / pipeline
Ano de origem19501934
Autor originalCarl SkaarGabriel Janka
Tipomoisture response testhardness test
Fonte seminalASTM D143-19. (2019). Standard test methods for small clear specimens of timber. ASTM International. link ↗ASTM D1037-21. (2021). Standard test methods for evaluating properties of wood-base fiber and particle panel materials. ASTM International. link ↗
Outros nomesdimensional change, anisotropic shrinkagewood hardness, resistance to indentation
Relacionados23
ResumoWood shrinkage is the dimensional change that occurs as wood loses moisture from green (freshly felled) to oven-dry condition. Wood shrinks anisotropically: tangentially (along growth rings) more than radially (from center to edge), and both more than longitudinally (along the grain). Measuring shrinkage percentages is essential for understanding wood drying behavior, predicting checking and warping, and selecting materials for applications sensitive to dimensional change (flooring, cabinetry, musical instruments).The Janka hardness test measures wood resistance to indentation and denting by forcing a steel ball into the wood surface under standard load. Developed by Gabriel Janka in 1934, the test is a simple, nondestructive indicator of wood durability, wear resistance, and suitability for flooring, furniture, and other wear-prone applications. Janka hardness is one of the most widely used wood property metrics in wood science and commerce.
ScholarGateConjunto de dados
  1. v1
  2. 2 Fontes
  3. PUBLISHED
  1. v1
  2. 2 Fontes
  3. PUBLISHED

Ir para a pesquisa Baixar slides

ScholarGateComparar métodos: Wood Shrinkage · Janka Hardness. Recuperado em 2026-06-19 de https://scholargate.app/pt/compare