Dureza Vickers×Nanoindentação×
ÁreaCiência dos materiaisCiência dos materiais
FamíliaProcess / pipelineProcess / pipeline
Ano de origem19221992
Autor originalSmith and SandlandWarren Oliver
TipoHardness testMeasurement method
Fonte seminalSmith, E., & Sandland, G. E. (1922). An accurate method of determining the hardness of metals with particular reference to high-hardness alloys. The Institution of Steel Engineers, 8, 623-641. link ↗Oliver, W. C., & Pharr, G. M. (1992). An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. Journal of Materials Research, 7(6), 1564-1583. DOI ↗
Outros nomesVickers hardness test, Vickers microhardness, HVnanoindentation, instrumented indentation, depth-sensing indentation
Relacionados33
ResumoVickers Hardness testing is a mechanical characterization technique for determining material hardness by pressing a diamond pyramid indenter into a material surface under controlled load and measuring the resulting indent dimensions. Invented by Smith and Sandland in 1922, Vickers hardness is applicable across an enormous hardness range (1-2000 HV) using the same indenter geometry at different loads. It is the most versatile hardness test, widely used in materials science, metallurgy, and quality control for assessing material strength and comparing alloy performance.Nanoindentation, or instrumented indentation, is a technique for measuring the hardness and elastic modulus of materials by pressing a hard probe into a sample surface and continuously recording load and penetration depth. Developed by Oliver and Pharr in 1992, nanoindentation enables measurement of mechanical properties of thin films, small volumes, and nanoscale structures with spatial resolution approaching micrometers. It is the standard tool in materials science for characterizing coatings, interfaces, and mechanical properties at the submicron scale.
ScholarGateConjunto de dados
  1. v1
  2. 3 Fontes
  3. PUBLISHED
  1. v1
  2. 3 Fontes
  3. PUBLISHED

Ir para a pesquisa Baixar slides

ScholarGateComparar métodos: Vickers Hardness · Nanoindentation. Recuperado em 2026-06-18 de https://scholargate.app/pt/compare