ScholarGate
Assistente

Comparar métodos

Examine os métodos selecionados lado a lado; as linhas que diferem ficam destacadas.

Dureza Janka×Encolhimento da Madeira×
ÁreaCiências florestaisCiências florestais
FamíliaProcess / pipelineProcess / pipeline
Ano de origem19341950
Autor originalGabriel JankaCarl Skaar
Tipohardness testmoisture response test
Fonte seminalASTM D1037-21. (2021). Standard test methods for evaluating properties of wood-base fiber and particle panel materials. ASTM International. link ↗ASTM D143-19. (2019). Standard test methods for small clear specimens of timber. ASTM International. link ↗
Outros nomeswood hardness, resistance to indentationdimensional change, anisotropic shrinkage
Relacionados32
ResumoThe Janka hardness test measures wood resistance to indentation and denting by forcing a steel ball into the wood surface under standard load. Developed by Gabriel Janka in 1934, the test is a simple, nondestructive indicator of wood durability, wear resistance, and suitability for flooring, furniture, and other wear-prone applications. Janka hardness is one of the most widely used wood property metrics in wood science and commerce.Wood shrinkage is the dimensional change that occurs as wood loses moisture from green (freshly felled) to oven-dry condition. Wood shrinks anisotropically: tangentially (along growth rings) more than radially (from center to edge), and both more than longitudinally (along the grain). Measuring shrinkage percentages is essential for understanding wood drying behavior, predicting checking and warping, and selecting materials for applications sensitive to dimensional change (flooring, cabinetry, musical instruments).
ScholarGateConjunto de dados
  1. v1
  2. 2 Fontes
  3. PUBLISHED
  1. v1
  2. 2 Fontes
  3. PUBLISHED

Ir para a pesquisa Baixar slides

ScholarGateComparar métodos: Janka Hardness · Wood Shrinkage. Recuperado em 2026-06-19 de https://scholargate.app/pt/compare