Differensiell scanning-kalorimetri×CALPHAD×
FagfeltMaterialvitenskapMaterialvitenskap
FamilieProcess / pipelineProcess / pipeline
Opprinnelsesår19641970
OpphavspersonE. S. WatsonLarry Kaufman
TypeMeasurement methodComputational method
Opprinnelig kildeWatson, E. S., O'Neill, M. J., Justin, J., & Brenner, N. (1964). A differential scanning calorimeter for quantitative differential thermal analysis. Analytical Chemistry, 36(7), 1233-1238. DOI ↗Kaufman, L., & Bernstein, H. (1970). Computer Calculation of Phase Diagrams. Academic Press. link ↗
AliasDSC, differential thermal analysis, thermal analysisCALPHAD method, computational thermodynamics
Relaterte33
SammendragDifferential Scanning Calorimetry (DSC) is a thermal characterization technique that measures the heat flow required to maintain a sample and an inert reference at the same temperature while both are heated or cooled. Invented by Watson, O'Neill, and colleagues in 1964, DSC directly quantifies enthalpy changes during phase transitions, crystallization, melting, and chemical reactions. It is the standard tool in materials science, chemistry, and pharmaceutical research for determining thermodynamic properties, thermal stability, and kinetics of thermal transitions.CALPHAD (CALculation of PHAse Diagrams) is a computational method for predicting thermodynamic equilibrium properties and phase diagrams of multicomponent alloys. Pioneered by Larry Kaufman in 1970, CALPHAD combines experimental and computational data to assess thermodynamic properties of phases and subsequently predict equilibrium conditions. It is the standard methodology in physical metallurgy and materials design for alloy development, process optimization, and understanding phase stability.
ScholarGateDatasett
  1. v1
  2. 3 Kilder
  3. PUBLISHED
  1. v1
  2. 3 Kilder
  3. PUBLISHED

Gå til søk Last ned lysbilder

ScholarGateSammenlign metoder: Differential Scanning Calorimetry · CALPHAD. Hentet 2026-06-19 fra https://scholargate.app/no/compare