Àrea superficial BET×Calorimetria Diferencial d'Escaneig×
CampCiència de materialsCiència de materials
FamíliaProcess / pipelineProcess / pipeline
Any d'origen19381964
Autor originalBrunauer, Emmett, TellerE. S. Watson
TipusMeasurement methodMeasurement method
Font seminalBrunauer, S., Emmett, P. H., & Teller, E. (1938). Adsorption of gases in multimolecular layers. Journal of the American Chemical Society, 60(2), 309-319. DOI ↗Watson, E. S., O'Neill, M. J., Justin, J., & Brenner, N. (1964). A differential scanning calorimeter for quantitative differential thermal analysis. Analytical Chemistry, 36(7), 1233-1238. DOI ↗
ÀliesBET analysis, nitrogen adsorption, surface area measurementDSC, differential thermal analysis, thermal analysis
Relacionats33
ResumBrunauer-Emmett-Teller (BET) Surface Area Analysis is a technique for measuring the specific surface area of solids by analyzing their nitrogen adsorption isotherms. Developed by Brunauer, Emmett, and Teller in 1938, BET theory extends monolayer adsorption (Langmuir) to multilayer adsorption, enabling quantification of surface area of porous and powdered materials. It is the industry standard for characterizing catalysts, adsorbents, pharmaceuticals, and porous materials, providing critical data for performance prediction and quality control.Differential Scanning Calorimetry (DSC) is a thermal characterization technique that measures the heat flow required to maintain a sample and an inert reference at the same temperature while both are heated or cooled. Invented by Watson, O'Neill, and colleagues in 1964, DSC directly quantifies enthalpy changes during phase transitions, crystallization, melting, and chemical reactions. It is the standard tool in materials science, chemistry, and pharmaceutical research for determining thermodynamic properties, thermal stability, and kinetics of thermal transitions.
ScholarGateConjunt de dades
  1. v1
  2. 3 Fonts
  3. PUBLISHED
  1. v1
  2. 3 Fonts
  3. PUBLISHED

Ves a la cerca Baixa les diapositives

ScholarGateCompara mètodes: BET Surface Area · Differential Scanning Calorimetry. Recuperat el 2026-06-20 de https://scholargate.app/ca/compare