Nanoindentation×Độ cứng Vickers×
Lĩnh vựcKhoa học vật liệuKhoa học vật liệu
HọProcess / pipelineProcess / pipeline
Năm ra đời19921922
Người khởi xướngWarren OliverSmith and Sandland
LoạiMeasurement methodHardness test
Công trình gốcOliver, W. C., & Pharr, G. M. (1992). An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. Journal of Materials Research, 7(6), 1564-1583. DOI ↗Smith, E., & Sandland, G. E. (1922). An accurate method of determining the hardness of metals with particular reference to high-hardness alloys. The Institution of Steel Engineers, 8, 623-641. link ↗
Tên gọi khácnanoindentation, instrumented indentation, depth-sensing indentationVickers hardness test, Vickers microhardness, HV
Liên quan33
Tóm tắtNanoindentation, or instrumented indentation, is a technique for measuring the hardness and elastic modulus of materials by pressing a hard probe into a sample surface and continuously recording load and penetration depth. Developed by Oliver and Pharr in 1992, nanoindentation enables measurement of mechanical properties of thin films, small volumes, and nanoscale structures with spatial resolution approaching micrometers. It is the standard tool in materials science for characterizing coatings, interfaces, and mechanical properties at the submicron scale.Vickers Hardness testing is a mechanical characterization technique for determining material hardness by pressing a diamond pyramid indenter into a material surface under controlled load and measuring the resulting indent dimensions. Invented by Smith and Sandland in 1922, Vickers hardness is applicable across an enormous hardness range (1-2000 HV) using the same indenter geometry at different loads. It is the most versatile hardness test, widely used in materials science, metallurgy, and quality control for assessing material strength and comparing alloy performance.
ScholarGateBộ dữ liệu
  1. v1
  2. 3 Nguồn tài liệu
  3. PUBLISHED
  1. v1
  2. 3 Nguồn tài liệu
  3. PUBLISHED

Đến trang tìm kiếm Tải xuống bản trình chiếu

ScholarGateSo sánh phương pháp: Nanoindentation · Vickers Hardness. Truy cập ngày 2026-06-18 từ https://scholargate.app/vi/compare