Диференційна сканувальна калориметрія×Раманівська деконволюція×
ГалузьМатеріалознавствоМатеріалознавство
РодинаProcess / pipelineProcess / pipeline
Рік появи19641928
Автор методуE. S. WatsonChandrasekhara Venkata Raman
ТипMeasurement methodAnalytical technique
Основоположне джерелоWatson, E. S., O'Neill, M. J., Justin, J., & Brenner, N. (1964). A differential scanning calorimeter for quantitative differential thermal analysis. Analytical Chemistry, 36(7), 1233-1238. DOI ↗Raman, C. V., & Krishnan, K. S. (1928). The scattering of light by molecules. Nature, 121(3048), 501-502. link ↗
Інші назвиDSC, differential thermal analysis, thermal analysisRaman deconvolution, Raman peak fitting, spectral analysis
Пов'язані33
ПідсумокDifferential Scanning Calorimetry (DSC) is a thermal characterization technique that measures the heat flow required to maintain a sample and an inert reference at the same temperature while both are heated or cooled. Invented by Watson, O'Neill, and colleagues in 1964, DSC directly quantifies enthalpy changes during phase transitions, crystallization, melting, and chemical reactions. It is the standard tool in materials science, chemistry, and pharmaceutical research for determining thermodynamic properties, thermal stability, and kinetics of thermal transitions.Raman Deconvolution is the mathematical decomposition of experimental Raman spectra into constituent peaks using spectral fitting algorithms. Building on Raman spectroscopy (discovered by C.V. Raman in 1928), Raman deconvolution resolves overlapping vibrational bands into individual component peaks, revealing detailed information about molecular bonds, crystal phases, strain, and defects. This quantitative analysis transforms raw Raman spectra into actionable chemical and structural insights, making it essential for materials characterization, quality control, and scientific discovery.
ScholarGateНабір даних
  1. v1
  2. 3 Джерела
  3. PUBLISHED
  1. v1
  2. 3 Джерела
  3. PUBLISHED

Перейти до пошуку Завантажити слайди

ScholarGateПорівняння методів: Differential Scanning Calorimetry · Raman Deconvolution. Отримано 2026-06-20 з https://scholargate.app/uk/compare