Просматривайте выбранные методы рядом; строки с различиями подсвечены.

Дифференциальная сканирующая калориметрия×Фазово-полевое моделирование×
ОбластьМатериаловедениеМатериаловедение
СемействоProcess / pipelineProcess / pipeline
Год появления19641958
Автор методаE. S. WatsonJohn W. Cahn
ТипMeasurement methodSimulation method
Основополагающий источникWatson, E. S., O'Neill, M. J., Justin, J., & Brenner, N. (1964). A differential scanning calorimeter for quantitative differential thermal analysis. Analytical Chemistry, 36(7), 1233-1238. DOI ↗Cahn, J. W. (1958). Free energy of a nonuniform system: Interfacial free energy. The Journal of Chemical Physics, 28(2), 258-267. DOI ↗
Другие названияDSC, differential thermal analysis, thermal analysisphase-field method, diffuse interface method
Связанные33
СводкаDifferential Scanning Calorimetry (DSC) is a thermal characterization technique that measures the heat flow required to maintain a sample and an inert reference at the same temperature while both are heated or cooled. Invented by Watson, O'Neill, and colleagues in 1964, DSC directly quantifies enthalpy changes during phase transitions, crystallization, melting, and chemical reactions. It is the standard tool in materials science, chemistry, and pharmaceutical research for determining thermodynamic properties, thermal stability, and kinetics of thermal transitions.Phase-Field Modeling (PFM) is a continuum computational method for simulating microstructure evolution, phase transitions, and interfacial dynamics without explicitly tracking moving boundaries. Developed from Cahn-Ginzburg-Landau theory in the 1950s, PFM represents distinct phases through continuous order parameters that vary smoothly over diffuse interfaces. This approach elegantly handles topological changes (nucleation, coalescence, pinch-off), complex interface geometries, and strongly coupled multiphysics. It is the dominant method for studying dendritic growth, spinodal decomposition, grain evolution, and reactive transport in materials science.
ScholarGateНабор данных
  1. v1
  2. 3 Источники
  3. PUBLISHED
  1. v1
  2. 3 Источники
  3. PUBLISHED

Перейти к поиску Скачать слайды

ScholarGateСравнение методов: Differential Scanning Calorimetry · Phase-Field Modeling. Получено 2026-06-19 из https://scholargate.app/ru/compare