Nanoindentacja×Skaningowa mikroskopia sił atomowych×Dynamic Light Scattering×Twardość Vickersa×
DziedzinaInżynieria materiałowaInżynieria materiałowaInżynieria materiałowaInżynieria materiałowa
RodzinaProcess / pipelineProcess / pipelineProcess / pipelineProcess / pipeline
Rok powstania1992198619641922
TwórcaWarren OliverGerd BinnigRobert PecoraSmith and Sandland
TypMeasurement methodImaging techniqueMeasurement methodHardness test
Źródło pierwotneOliver, W. C., & Pharr, G. M. (1992). An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. Journal of Materials Research, 7(6), 1564-1583. DOI ↗Binnig, G., Quate, C. F., & Gerber, C. (1986). Atomic force microscope. Physical Review Letters, 56(9), 930-933. DOI ↗Pecora, R. (1964). Spectral distribution of scattered light from a suspension of particles. Physica, 30(11), 2055-2070. link ↗Smith, E., & Sandland, G. E. (1922). An accurate method of determining the hardness of metals with particular reference to high-hardness alloys. The Institution of Steel Engineers, 8, 623-641. link ↗
Inne nazwynanoindentation, instrumented indentation, depth-sensing indentationAFM, scanning probe microscopy, nanoindentation microscopyDLS, photon correlation spectroscopy, particle size measurementVickers hardness test, Vickers microhardness, HV
Pokrewne3333
PodsumowanieNanoindentation, or instrumented indentation, is a technique for measuring the hardness and elastic modulus of materials by pressing a hard probe into a sample surface and continuously recording load and penetration depth. Developed by Oliver and Pharr in 1992, nanoindentation enables measurement of mechanical properties of thin films, small volumes, and nanoscale structures with spatial resolution approaching micrometers. It is the standard tool in materials science for characterizing coatings, interfaces, and mechanical properties at the submicron scale.Atomic Force Microscopy (AFM) is a scanning probe technique that measures nanoscale surface topography and mechanical properties by monitoring interactions between a sharp cantilever tip and a sample surface. Invented by Gerd Binnig in 1986 as an extension of scanning tunneling microscopy, AFM requires neither electrical conductivity nor vacuum operation, making it applicable to virtually any material. It provides three-dimensional topographic maps with sub-nanometer vertical resolution and lateral resolution approaching nanometers, along with simultaneous measurements of mechanical, electrical, and chemical properties.Dynamic Light Scattering (DLS), also known as Photon Correlation Spectroscopy (PCS), is an analytical technique for determining the size and size distribution of particles suspended in fluids by analyzing the time-dependent intensity fluctuations of scattered laser light. Developed by Robert Pecora in 1964, DLS exploits the Brownian motion of particles: smaller particles move faster, causing faster intensity fluctuations; larger particles move slower, causing slower fluctuations. By correlating intensity over time, particle size is deduced. DLS is rapid, non-destructive, and requires minimal sample volume, making it the standard technique for characterizing nanoparticles, proteins, colloids, and emulsions.Vickers Hardness testing is a mechanical characterization technique for determining material hardness by pressing a diamond pyramid indenter into a material surface under controlled load and measuring the resulting indent dimensions. Invented by Smith and Sandland in 1922, Vickers hardness is applicable across an enormous hardness range (1-2000 HV) using the same indenter geometry at different loads. It is the most versatile hardness test, widely used in materials science, metallurgy, and quality control for assessing material strength and comparing alloy performance.
ScholarGateZbiór danych
  1. v1
  2. 3 Źródła
  3. PUBLISHED
  1. v1
  2. 3 Źródła
  3. PUBLISHED
  1. v1
  2. 3 Źródła
  3. PUBLISHED
  1. v1
  2. 3 Źródła
  3. PUBLISHED

Przejdź do wyszukiwania Pobierz slajdy

ScholarGatePorównaj metody: Nanoindentation · Atomic Force Microscopy · Dynamic Light Scattering · Vickers Hardness. Pobrano 2026-06-19 z https://scholargate.app/pl/compare