Jankova tvrdost×Rentgenová densitometrie×
OborLesnictvíLesnictví
RodinaProcess / pipelineProcess / pipeline
Rok vzniku19342005
TvůrceGabriel JankaGabriel Gazo
Typhardness testmeasurement method
Původní zdrojASTM D1037-21. (2021). Standard test methods for evaluating properties of wood-base fiber and particle panel materials. ASTM International. link ↗Hansmann, C., Wimmer, R., & Gindl, W. (2007). Assessing damage in wood-polymer composites by depth-sensing indentation. Composites Part A, 38(6), 1502–1508. link ↗
Další názvywood hardness, resistance to indentationwood density, radiography
Příbuzné33
ShrnutíThe Janka hardness test measures wood resistance to indentation and denting by forcing a steel ball into the wood surface under standard load. Developed by Gabriel Janka in 1934, the test is a simple, nondestructive indicator of wood durability, wear resistance, and suitability for flooring, furniture, and other wear-prone applications. Janka hardness is one of the most widely used wood property metrics in wood science and commerce.X-ray densitometry is a nondestructive method for measuring wood density, microdensity profiles, and ring-by-ring density variation in wood samples using X-ray image analysis. The method uses attenuation of X-rays passing through wood to quantify mass per unit volume. It enables rapid assessment of wood quality without destroying material, making it valuable for research, timber grading, and genetic selection programs.
ScholarGateDatová sada
  1. v1
  2. 2 Zdroje
  3. PUBLISHED
  1. v1
  2. 2 Zdroje
  3. PUBLISHED

Přejít na hledání Stáhnout prezentaci

ScholarGatePorovnat metody: Janka Hardness · X-ray Densitometry. Získáno 2026-06-18 z https://scholargate.app/cs/compare