Nanoindentation
Nanoindentation, or instrumented indentation, is a technique for measuring the hardness and elastic modulus of materials by pressing a hard probe into a sample surface and continuously recording load and penetration depth. Developed by Oliver and Pharr in 1992, nanoindentation enables measurement of mechanical properties of thin films, small volumes, and nanoscale structures with spatial resolution approaching micrometers. It is the standard tool in materials science for characterizing coatings, interfaces, and mechanical properties at the submicron scale.
Allikakirje
Tsiteeringud kopeeritud meetodi allikakirjest sõna-sõnalt. Nendest ei saa järeldada väidete tasemel kinnitust.
- Oliver, W. C., & Pharr, G. M. (1992). An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. Journal of Materials Research, 7(6), 1564-1583. · DOI 10.1557/JMR.1992.1564
- Fischer-Cripps, A. C. (2004). Nanoindentation (2nd ed.). Springer-Verlag. · URL
- Hay, J. L., & Crawford, B. (2011). Measuring substrate-independent modulus of thin films. Journal of Materials Research, 26(6), 727-738. · DOI 10.1557/jmr.2011.8
Kureeritud väited
Väited on salvestatud tõendite registrisse, igal oma hinnanguga.
See vaade ei loo väite hinnangut, kui registris seda pole.
Seotud meetodid
Genereeritud meetodigraafist ja kuvatud masina soovitatud seostena – väiteid ei järeldata.